Dana89
Well-Known Member
- Joined
- Nov 9, 2014
- Messages
- 294
- Reaction score
- 252
I have my oils melting and my lye water cooling and I need last minute advice.
I bought Blackberry Bling Bling FO from NG and have great colors to go with it.
The problem is while the description says perfect pour-no R or A several customers said it caused serious ricing. Need advice on how to prevent this or at least make it to where it is not too bad. What would be the best temp? Should I use full water? My solution right now is 50/50.
My recipe
40% Lard
20% Olive
20% coconut
10% shea
5% castor
5% S. Almond
SF 7%
Lye-8.90
Water at 38% 24.70
This recipe has a lot of hard oils and I have never made it before. The oils are all togeather melting so I really cannot change it. I could add to it and re-calculate my lye
The total oils are 65 oz.
Thanks in advance.
l
I bought Blackberry Bling Bling FO from NG and have great colors to go with it.
The problem is while the description says perfect pour-no R or A several customers said it caused serious ricing. Need advice on how to prevent this or at least make it to where it is not too bad. What would be the best temp? Should I use full water? My solution right now is 50/50.
My recipe
40% Lard
20% Olive
20% coconut
10% shea
5% castor
5% S. Almond
SF 7%
Lye-8.90
Water at 38% 24.70
This recipe has a lot of hard oils and I have never made it before. The oils are all togeather melting so I really cannot change it. I could add to it and re-calculate my lye
The total oils are 65 oz.
Thanks in advance.
l